Differential Scanning Calorimeter LDSC-A14 operates within a temperature range of -40 to 600°C, ensuring reliable thermal analysis. A heating rate of 0.1 to 100°C per minute allows precise control of heat transition measurements. The DSC resolution of 0.01μW enhances sensitivity for accurate detection of heat flow variations. A metal U-shape furnace body ensures measurement stability and repeatability. Ideal for polymer development, phase transition studies, and quality control applications.
| Temperature Range | -40 to 600°C |
| Heating Rate | 0.1 to 100°C/min |
| Temperature Resolution | 0.01°C |
| Temperature Fluctuations | ±0.01°C |
| Temperature Repeatability | ±0.1°C |
| Constant Temperature Time | Program setting up to 24h |
| DSC Range | 0 to ±600mW |
| DSC Noise | 0.01μW |
| DSC Resolution | 0.01μW |
| Atmosphere Control Gas | Nitrogen, Oxygen (automatic switching) |
| Gas Flow Rate | 0 to 300mL/min |
| Gas Pressure | 0.2MPa |
| Control Mode | Rising, cooling, constant temperature (fully automatic) |
| Curve Scanning | Rising scan, cooling scan |
| Gas Flow Control | Built-in digital flow meter & software-controlled |
| Display | 7-inch LCD touch screen (24-bit) |
| Data Interface | Standard USB connector |
| Software | Professional control operating software |
| Thermocouples | 3 sets: sample temperature, furnace temperature, internal ambient temperature |
| Cooling Device | Semiconductor refrigeration |
| Power Supply | AC220V/50Hz |
| Machine Dimensions | 500 × 430 × 300 mm |
| Packing Dimensions | 620 × 530 × 500 mm |
| Net Weight | 25 kg |
| Gross Weight | 30 kg |
High-resolution thermal analysis
Bilateral operation control system
Multi-curve data analysis software
Automatic gas flow regulation
Built-in digital flow meter
Semiconductor refrigeration system
7-inch LCD touchscreen display
Standard USB data interface
Supplied with water bath
Our Differential Scanning Calorimeter LDSC-A14 is designed to analyze heat transition behaviour under controlled temperature conditions. It is widely used in polymer development, pharmaceuticals, food science, and material testing laboratories.
Accessory Name | Quantity |
Host Instrument | 1 pc |
Water Bath | 1 pc |
CD | 1 pc |
Data Line | 1 pc |
Power Line | 1 pc |
Aluminum Crucibles | 100 pcs |
Ceramic Crucibles | 100 pcs |
Pure Tin Grains | 1 bag |
Fuse 4A | 5 pcs |
Accessory Name | Quantity |
Crucible Aluminum with Cap | 300 pcs |
Press | 1 pc |
Labtron Equipment Ltd., Quatro House, Lyon Way, Camberley, Surrey GU16 7ER United Kingdom
Email: info@labtron.com Whatsapp: +44 73 4441 2688 Phone: +44 2080 043608